LATEST NEWS
-
Sep 26th 2025A spray trace is caused by the melt flowing too fast in plastic injection molding, generally serpentine. Causes: (1) The gate size ...
-
Sep 24th 2025It refers to the surface of the part that can be peeled off layer by layer. Causes: (1) Mixing other incompatible polymers (2) E...
-
Sep 22nd 2025It means that excess plastic is present on the mold parting or ejector part. Causes: (1) Insufficient clamping force (2) The mol...
-
Sep 19th 2025The burn marks in plastic injection molding are that the gas in the cavity cannot be removed in time, resulting in blackening at the end ...
-
Sep 17th 2025Brittleness is that the plastic part is easily cracked or broken in some place Causes: (1) Dry conditions are not suitable; use exc...
-
Sep 15th 2025Air traps are where air is trapped in the cavity to create bubbles in the part during plastic injection molding. Causes: It is caused ...
-
Sep 12th 2025Short shots are a phenomenon in which the mold cavity cannot be completely filled. Plastic Injection Molding-Short Shots Causes: (...
-
Sep 10th 2025The process involved many steps until a final prototype or product is fabricated. The first step in prototyping of plastic injection mold...
-
Sep 8th 2025Injection molding is ideal for making precise silicone rubber parts from LSR. It offers parts with accurate dimensions, intricate design,...
-
Sep 5th 2025Different production volumes are also an essential factor in the cost of injection molding. Moreover, the production volume influences th...
-
Sep 3rd 2025Generally, the injection molding process has no fixed cost for every application. Custom injection molding cost has a varying value that ...
-
Sep 1st 2025Cooling is a critical phase in plastic injection molding, directly influencing production efficiency, product quality, and cost-effective...